Published January 1, 2010 | Version v1
Journal article Open

Improving the direct borohydride fuel cell performance with thiourea as the additive in the sodium borohydride solution

  • 1. Kocaeli Univ, Dept Mech Engn, TR-41380 Kocaeli, Turkey
  • 2. Energy Inst, TUBITAK Marmara Res Ctr, TR-41470 Gebze, Kocaeli, Turkey

Description

In this study, the effects of the additive thiourea (TU) have been investigated under steady state/steady-flow and uniform state/uniform-flow systems with the aim of minimizing the anodic hydrogen evolution on Pd in order to increase the performance of a direct borohydride fuel cell. The fuel cell has consisted of Pd/C anode, Pt/C cathode and Na+ form Nafion membrane as the electrolyte. There has been a small improvement in peak power density and fuel utilization ratio by addition of TU (1.6 x 10(-3) M) into the sodium borohydride solution; the peak power densities of 14.4 and 15.1 mW cm(-2), and fuel utilization ratios of 21.6% and 23.2% have been obtained without and with TU, respectively. (C) 2010 Professor T. Nejat Veziroglu. Published by Elsevier Ltd. All rights reserved.

Files

bib-b0e485e3-04e6-4341-9862-91b80670d585.txt

Files (220 Bytes)

Name Size Download all
md5:4130b9941f62c8dc8c73a7f33c1d5aa5
220 Bytes Preview Download