Published January 1, 2011 | Version v1
Journal article Open

Fe Containing ZSM-5 Zeolite as Catalyst for Wet Peroxide Oxidation of Orange II

  • 1. Ege Univ, Izmir, Turkey
  • 2. Izmir Inst Technol, Izmir, Turkey

Description

This study presents the catalytic performances of iron containing ZSM-5 zeolites, prepared by ion exchange or hydrothermal synthesis, in catalytic Fenton-like oxidation of Orange II in aqueous solution. The catalyst, ZSM-5 zeolite with Si/Al ratio of 42 loaded with iron by ion exchange, showed the highest activity. The decolorization of 99.7 percent, degradation of 87.0 percent and COD removal of 81.2 percent were achieved over this catalyst at an initial pH of 3.5. Incorporation of iron into ZSM-5 structure increased its catalytic activity. The hydrothermally prepared FeZSM-5 catalyst was more stable against leaching at low pH value due to the iron being in the framework.

Files

bib-7ba4bfd8-0224-444b-862d-c40b76e5cf8d.txt

Files (213 Bytes)

Name Size Download all
md5:c6c4e18fe2c108979f2f273cca4f38ee
213 Bytes Preview Download