The Utilization of Waste Magnesite in the Production of the Cordierite Ceramic

   Askin, Aysegul; Tatar, Ilknur; Kilinc, Sule; Tezel, Ozge

Cordierite ceramics comprises MgO as the main ingredient. In this work, cordierite composition was prepared with raw magnesite (CR) and with waste magnesite (CW) generated during the magnesite processing, sintered at various temperatures, between 1250-1350 degrees C, and heating rates, and then samples were analyzed with DTA, XRD and their bulk density, water absorption and porosity were determined. The cordierite composition prepared with waste magnesite and sintered at 1325 degrees C and 3 degrees C/min heating rate, produced a single-phase cordierite with 1.64 g/cm3 bulk density, and 36.5%, and 22.5% porosity and water absorption, respectively, which demonstrates its suitability for the cordierite production. (C) 2017 The Authors. Published by Elsevier Ltd.

Dosyalar (208 Bytes)
Dosya adı Boyutu
bib-6ea25516-9aa5-4697-8944-73d7a393d49d.txt
md5:d2e0a9aa3afb832202ec30403e5484e1
208 Bytes İndir
89
10
görüntülenme
indirilme
Görüntülenme 89
İndirme 10
Veri hacmi 2.1 kB
Tekil görüntülenme 79
Tekil indirme 10

Alıntı yap